copper flotation tests rougher

Enquiry ›

Study of solid and liquid behavior in large copper… pdf

Ammonium Bromide, for floatable solid recovered in the concentrate Cu-64, and for non-floatable solid in three particle size classes (coarse: >150 µm, ... a 130 m3 industrial flotation cell of the rougher circuit at El Teniente Division, Codelco-Chile. 1. INTRODUCTION. Froth ... Experimental tests were developed for water and...

GET MORE INFORMATION

Evaluating Copper Rougher-Scavenger Flotation…

17 Mar 2017 ... A modal examination of the products produced by the copper flotation rougher-scavenger circuit reveal important information regarding the limits to the ... Let's discusses various aspects of rougher flotation circuit performance and how to evaluate its results . ... Rougher Scavenger Circuit Tested for Kinetics.

GET MORE INFORMATION

Froth flotation circuit design and basic testwork…

Froth flotation can recover many minerals, but requires laboratory testing to maximize retention and seperate ... The objective of passing through the rougher and scavenger flotation circuits is to maximise recovery of the desired minerals into relatively low grade concentrates that may typically contain 5-15 weight percent of...

GET MORE INFORMATION

1 Froth Flotation – Fundamental Principles… pdf

(e) Enrichment Ratio. Table 1: Grade/recovery performance of a hypothetical copper ore flotation process. Product. % Weight. % Cu Assay. Feed. 100. 2.09 ..... 12: One possible configuration for a Rougher/Cleaner/Scavenger flotation circuit. Rougher. Scavenger. Cleaner. Rougher Froth. Cleaner Tails + Scavenger Froth.

GET MORE INFORMATION

Separation efficiency improvement of a low grade… pdf

Separation efficiency improvement of a low grade copper-gold flotation circuit. David seaman / Peter manton / Paul griffin. Newcrest Mining, Australia. Abstract. Newcrest's ... evaluation of key streams, flotation circuit surveys, floatability component model fitting and simulation, and the application of dilute batch flotation tests.

GET MORE INFORMATION

Flotation separation of copper sulphides from…

Flotation behaviour of arsenic and non-arsenic copper minerals at finer sizes was investigated by grinding and flotation tests conducted in the on-site laboratory at Rosebery on samples taken from the copper rougher concentrate stream. The average assay of the copper rougher concentrate was 9% Cu, 3600 ppm As and...

GET MORE INFORMATION

Preliminary Metallurgical Results Indicate Good Gold… pdf

6 Dec 2011 ... The test work consists of single and sequential leaching tests for copper and gold, gravity separation tests ... Sequential sulphuric acid – cyanidation bottle roll leach tests on oxide material indicate copper .... subjected to a total of 10 rougher concentrate flotation tests to evaluate variation in grind size and.

GET MORE INFORMATION

Flotation Technology Brochure - FL pdf

flotation concentration test in one of the many labs in our Technology Center. 3. FL is the leader in ... 250m3 Wemco Cells installed in a Copper plant in Mexico. 4. WEMCO® Flotation. Machines have the .... cell is a true workhorse for rougher, rougher scavenger and cleaner scavenger applications. The Dorr-Oliver...

GET MORE INFORMATION

the evaluation of a copper flotation plant performance by… pdf

In this study the performance evaluation study of Georgia Madneuli Copper Ore flotation plant was performed using the data ... The laboratory flotation tests were performed to obtain the optimum flotation conditions. For this ... volumetric size of the cells in the rougher, scavenger and cleaner circuits are 6.3 m3,. * Hacettepe...

GET MORE INFORMATION

Improving the Recovery of Miduk Copper Complex Coarse… pdf

3 Dec 2011 ... 2: Three vertical zones of deposit of Miduk copper lay down. 4. Method Table 1: Characteristics of the average feed ore sample. (a) laboratory Flotation Tests. Laboratory flotation tests were carried out to evaluate the response of the chalcopyrite and chalcocite rougher flotation to a change in distribution of.

GET MORE INFORMATION

Froth Floatation Process - YouTube

5 May 2010 ... Follow us at: https://plus.google.com/+tutorvista/ Check us out at Froth Floatation Proce...

GET MORE INFORMATION

flotation optimization and variability testing… pdf

rougher flotation. The type 2 samples were more sensitive to primary grind size, compared to the other two types of samples. Four stages of cleaning at pH >11.5 with rougher concentrate regrinding obtained a product grade higher than 25% Cu. Locked cycle testing using a flowsheet as shown below confirmed that the type...

GET MORE INFORMATION

Particle size distribution effects considered for… pdf

A single-stage batch flotation test, which can be used to gain an indication/ranking of the expected recovery of different ore types, or used to derive model parameters for subsequent flotation modelling of performance in a multistage flow sheet. • A rougher/cleaner test in which the concentrates are repeatedly floated to...

GET MORE INFORMATION

Froth flotation - Wikipedia

The rougher flotation step is often followed by a scavenger flotation step that is applied to the rougher tailings. The objective is to recover any of the target minerals that were not recovered during the initial roughing stage. This might be achieved by changing the flotation conditions to make them more rigorous than the initial...

GET MORE INFORMATION

Flotation experiment research on a polymetallic sulfide… pdf

help remove more gangue and metal. The mesh of grind test was conducted by rougher the copper/lead bulk flotation with 1500 g/t of lime, 1000g/t of Zinc sulfate, 500 g/t of sodium sulfate, 40 g/t of Z-200, 40 g/t of butylamine aerofloat, and 20 g/t of #2 oil (specific conditions by inspection was used after inspection in the next.

GET MORE INFORMATION

Concentrator Process Development Phase IV Flotation… pdf

19 Dec 2008 ... Figure 11: Copper Recovery and Mass Rejection Rates for Rougher Scoping Flotation Tests..................... 30. Figure 12: Copper and Zinc Grades in Concentrate for Rougher Scoping Flotation Tests............................ 30. Figure 13: Copper-Zinc Separation Efficiency for Rougher Scoping Flotation Tests .

GET MORE INFORMATION

Mineral Flotation - International Mining

1 Nov 2011 ... Flotation has been at the heart of the mineral processing industry for over 100 years, addressing the 'sulphide' problem of the early 1900s, and continues to provide one of the most important tools in mineral separation today. The realisation of the effect of a minerals hydrophobicity on flotation all those...

GET MORE INFORMATION

Developing a Bulk Circuit Suitable for Chalcopyrite ... - UQ… pdf

the objective was to apply bulk rougher flotation of both the copper minerals and pyrite for the copper-gold-pyrite ore at ... A standard test with a sequential circuit was applied to the same ore for comparison. The chalcopyrite and pyrite losses in the tailing from the rougher circuit were the same for both bulk and sequential...

Optimization of Rougher Flotation Parameters of the… pdf

Response surface plots showing the effect of two variables on recovery of copper (other two variables are held at center level): (a) pH and solid content and (b) pH and ratio Z11 to mer- captobenzothiazole when tap water was used in flotation tests. The performance of rougher flotation of the Sarcheshmeh copper ore was...

GET MORE INFORMATION

Effect of Primary Grind Size on Copper Flotation Rougher…

19 Mar 2017 ... An example of a copper metallurgy study where the effect of primary grind on rougher flotation each of the GeoMetallurgical samples was investigated. A simple economic study was conducted on these copper flotation results, using typical power costs and a net smelter revenue value for copper of 90 cents.

GET MORE INFORMATION

An investigation into the recovery of Molybdenum, Copper… pdf

The testwork investigated the flotation options for the recovery of copper, molybdenum and silver minerals from the CUMO property in Idaho. The scope of the program involved sample preparation, grindability testing, mineralogical characterization via QEMSCAN analysis, rougher kinetics testing, batch cleaner testing,...

GET MORE INFORMATION

The Testing and Concentration of a Low Grade… pdf

In two of the tests performed, the copper rougher concen- trate was placed in a 250 gram cell and cleaned up to remove the major portion of the small amount of pyrrhotite which was floated with the chalcopyrite. A flow sheet showing the steps taken in testing the ore is given on page 16. FLOTATION TESTS NO.1 and 2.

The Use of Design of Experimentation Software in Applied… pdf

30 Sep 2013 ... Powder Metallurgy & Mining. The Use of Design of Experimentation Software in Applied Flotation. Testing. Corby G Anderson1* and Todd S Fayram2 ..... Almost. Table 11: Flotation Recovery Optimization Testing Results. Test. Co Rec.,. %. Cu Rec.,. %. Au Rec.,. %. Co %,. Rougher. Conc. Grade. Cu %,.

GET MORE INFORMATION

Flotation of copper sulphides assisted by high… pdf

rougher concentrate. Rodrigues et al. (2005). Brazil/copper. Investigation of a copper flotation circuit aiming to identify copper losses on fine fraction. Flotation circuit changes were proposed, .... Compar-. Fig. 3. Schematic representation of the configuration of a standard mill test and details of the flotation cell and froth. Fig. 4.

GET MORE INFORMATION

The behaviour of minerals in sulphide flotation… pdf

ing a variety of copper and lead-zinc sulphide ores. The plant work has been supplemented where necessary with particular laboratory and pilot- scale tests. ..... Equation. (5) is simply the trad- itional first-order rate equation for the flotation process. However, if a rougher/scavenger bank is con- sidered, the value of the rate...

GET MORE INFORMATION

Flotation Testwork - ALS Global pdf

2 |Flotation Testwork. Introduction. ALS Metallurgy is part of the ALS Group, a diversified and global analytical laboratory and testing services company. ALS Metallurgy is the ... Base metals - copper, cobalt, lead, zinc, molybdenum, manganese ... Flotation testwork is carried out from rougher, cleaner and locked cycle tests...

GET MORE INFORMATION

Simulation of Flotation Plants - Outotec

Figure 3: Buenavista del Conre plant II rougher line cumulative Cu grade and recovery measurement and simulations. For a greenfield plant design, the flotation models are typically based on kinetic laboratory tests carried out both for the rougher and cleaner stages. It is also common to carry out closed loop locked cycle...

GET MORE INFORMATION

Pyrite-Gold Recovery in Copper Rougher Flotation… pdf

at the head of copper flotation (copper rougher feed) and after regrinding of the copper rougher tailings, before gold/pyrite selective flotation. Also, different collector regimes, involving sodium iso-butyl xanthate (SIBX) and. N-butoxycarbonyl-nbutyl thionocarbamate (XD5002), have been tested. It was found that aeration of...

GET MORE INFORMATION

Copper Flotation - 911 Metallurgist

19 Mar 2017 ... Although a clean rougher tailing can often be achieved at 65-mesh the copper mineral is not liberated sufficiently to make a high grade copper concentrate, thus some form of regrinding is necessary on the rougher flotation copper concentrate. It is not unusual to grind the rougher flotation concentrate to...

GET MORE INFORMATION

The application of flotation test work to plant design and… pdf

Process Flow Diagram. Milling. Thickener. Rougher float. Re-cleaners. (2/3 stage). Cleaner float. Attritioners. To secondary float. Final concentrate. Tailings. Tailings ... Reagents. – Copper Sulphate. – SIBX. – Depressant (CMC). – Frother (Dow 200). • Test parameters. – Solids Concentration. – Frother Concentration.

GET MORE INFORMATION

Flotation Test of a High Silica Copper Oxide Ore in… pdf

of size mixing. The effect of different dosage of lime on copper flotation was researched. In roughing process for 4 minutes, the grinding fineness of70% -0.074mm, 1000g/t sodium sulfide, 150g/t butyl xanthate, and 30g/t terpenic oil were used to conduct the tests. Flotation indexes of rough concentrate were obtained with the.

GET MORE INFORMATION

Advanced Modelling for Scale-Up of Batch Flotation… pdf

standardised batch flotation test called the MFT. The work is part of the FLEET program, ... To date, the methodology has been applied with success at several industrial plants, encompassing copper, gold, nickel, iron, lead, zinc and coal operations. .... The test sample consisted of rougher feed collected in the plant using.

Flotation of mixed copper oxide and sulphide… pdf

At a blend of 70% sulphide ore and 30% oxide ore, the rougher scavenger copper recovery was as high as .... The rough- er scavenger flotation test was conducted over six stages. Before each stage of flotation, 1 min conditioning time was allowed after. 1 AM28 is the trade name of one of Ausmelt's hydroxamate collectors.

GET MORE INFORMATION

Metallurgical Test Work Update, Oman Copper… pdf

6 Feb 2017 ... Test work also indicates relatively low equipment liner and grinding media wear due to low abrasion rates. • Initial rougher flotation test work indicated potential recoveries of around. 95% at moderate grind sizes. • Rougher cleaner flotation at 38microns indicated that a saleable copper concentrate of over...

GET MORE INFORMATION

Size dependent gold deportment in the products of copper… pdf

Once the deportment of gold across the rougher separation was understood, and reasons for poor gold recovery identified, strategies to increase gold recovery were tested. Size dependent gold deportment in the products of copper flotation and methods to increase gold recovery by G. Small, A. Michelmore, and S. Grano*.

GET MORE INFORMATION

Improved Cleaner CIrCuIt performanCe at the degrussa… pdf

20 Jan 2016 ... early after commissioning, it was identified that the flotation capacity in the all-mechanical cleaner circuit was not sufficient. In order to improve recovery, the tail from the cleaner scavenger was sent back to feed the rougher scavengers. test-work was done on-site to evaluate the possibility of using a flotation...

GET MORE INFORMATION

Low pH Trial in the Ernest Henry Mining Copper Rougher… pdf

17 Jul 2013 ... 1 – Copper grade / recovery curves for copper flotation tests completed on SAG feed samples ground with forged and 18 percent chrome grinding media with varying pH (Kinal, 2006). REDUCED FLOTATION PH. Rougher circuit pH reduction trial. In March 2012 EHM ran a plant trial over three days where...

GET MORE INFORMATION

Beneficiation Tests on Taivaljärvi Ore - Sotkamo Silver… pdf

2 May 2011 ... The cell sizes of 4 and 2,5 were used in cleaner flotation stages. The used reagents in lead flotation were zinc sulphate (ZnSO4) and Aerophine 3418A in rougher flotation and sodium cyanide (NaCN) and Aerophine 3418A in cleaner stages. Reagents used in zinc flotation were copper sulphate (CuSO4)...

GET MORE INFORMATION

Up-scaling of froth flotation equipment - TU Delft… pdf

7 Jul 2014 ... Laminar flow zone of pulp between the mixing and froth zones of the flotation cell, through which loaded bubbles rise to the top of the cell. Responses: Test results being compared in a factorial design test. Rougher flotation: First stage of the flotation process, aiming for a low grade of the valuable metal in...

GET MORE INFORMATION

Constancia Project Process Plant Design and Start Up -… pdf

Pilot scale flotation testing was also completed during the DFS. Approximately 25 t of feed material was fed to the pilot plant to confirm laboratory metallurgical design criteria and produce material for: rougher concentrate regrinding testing, copper concentrate rheology, thickening and filtration testing, and final tailings...

GET MORE INFORMATION